FOR EXISTING CUSTOMERS
Enter the access code we sent you and check your mold’s machining progress at any time — every step photographed on the shop floor the same day.
SERVICE
Hollow parts in food-contact and industrial grades, produced on our own lines with wall-thickness control and per-lot documentation.
SERVICE
Hollow parts in food-contact and industrial grades, produced on our own lines with wall-thickness control and per-lot documentation.
| Process | Equipment | What it means for your part |
|---|---|---|
| Blow molding | In-house lines | Bottles, jerrycans, drums and hollow industrial parts in HDPE, LDPE and PP. |
| Multi-layer | Co-extrusion | PE / EVOH / PA barrier structures without a separate laminate. |
| Mold | In-house mold shop | Blow molds cut and finished here, so the cavity matches the parison we actually extrude. |
| Quality | Wall-thickness and weight checks | Measured per part, not per batch – this is where blow molding usually fails. |
| Documentation | MTR and CoO per lot | Batch traceability and food-contact documentation issued with the shipment. |
Blow molding is a different buy from injection molding. The wall of the part is extruded, not cut from a runner, so thickness comes out of the molds and the extrusion control rather than the cavity fill. We run extrusion and blow molding lines in house, cut and finish the blow molds in our own mold shop, and measure wall thickness and weight per part instead of per batch. Bottles, jerrycans, drums and hollow industrial parts come out of the same 1,200 m² site that builds the injection molds.
Resin is melted in the extruder and pushed through a die to form a tube, called the parison. The parison is transferred into the open mold, the mold closes, and compressed air inflates it against the cavity wall. The part cools inside the mold, the mold opens, and the flash and neck are trimmed off. Five things decide the result: parison weight, parison temperature, mold temperature, blow ratio and cooling time. Ignore any one of them and the parts look right and weigh wrong.
| Stage | What happens | What we control |
|---|---|---|
| Extrusion | Resin is melted and a controlled-weight parison is formed | Parison weight tolerance, die gap and the temperature profile |
| Transfer | The parison moves into the open mold without sagging | Transfer speed and drop time |
| Blowing | The mold closes and air inflates the parison to shape | Blow rate, blow ratio and air pressure |
| Cooling | The part solidifies while held in the cavity | The mold cooling circuit and the cooling time |
| Trimming | Flash, neck and finishing are separated from the body | Neck finish, thread geometry and the sealing band |
| Material | Typical behavior | What it means for your tool |
|---|---|---|
| HDPE (food grade) | Stiff, chemically resistant, near-zero water uptake | The usual choice for oil, detergent and milk bottles |
| LDPE | Soft and flexible compared with HDPE | Works for squeeze bottles and closures where the body has to flex |
| PP | Recyclable, semi-crystalline, good fatigue behavior | Common for drums and jerrycans, and the usual resin for a recyclable pack |
| PE / EVOH / PA multi-layer | A barrier layer inside a PE structure | Co-extrusion gives barrier performance without adding a separate laminate |
Blow molding is usually limited by wall thickness, not by tolerance. Typical linear shrinkage for HDPE is around 1.5–2.5% depending on the grade, the mold temperature and the cooling time, and PP usually sits a little higher. Your drawing should therefore state the dimensions as measured at room temperature after conditioning, not as they come off the line.
Typical minimum walls are 1.0–1.5 mm for small containers and 2–3 mm for larger drums, depending on the part size and the load it carries. Where a dimension cannot be molded, the normal route is a machined neck finish. Thread geometry, closure torque and the sealing band are cut on the neck rather than formed in the mold, so they hold regardless of body shrinkage.
Each cavity needs its own neck and flash handling, so the number of cavities depends on the neck geometry and the machine layout rather than on the size of the body. Multi-cavity tools are normal, but every extra cavity adds cooling and trimming complexity. Draft is required on every surface that releases from the mold, and the shoulder is the first place to look when a part scuffs or sticks.
Cooling sets the cycle time in blow molding. A mold with an unbalanced cooling circuit produces a part that is still soft when it is trimmed, and the difference shows up as an oval body, a warped neck or a weight spread across the batch. We measure weight per part because it catches a cooling fault before a customer does.
| Symptom | Typical cause | What we change |
|---|---|---|
| Short shot or incomplete fill | Parison too light, mold not fully closed, or low blow pressure | Increase parison weight, check mold closure and air pressure |
| Flash at the parting line | Damaged parting face, worn pinch-off, or excess pressure | Repair the pinch-off and dress the parting face |
| Uneven wall thickness | Uneven cooling, wrong parison weight, or an off-center preform | Rebalance the cooling and correct the parison |
| Oval body or warpage | The part is trimmed before it has cooled enough | Extend the cooling time and check mold temperature control |
| Weak or split neck | Cold neck, or the parison is too cold when it reaches the mold | Control the neck region separately from the body |
| Weld lines | Not applicable in blow molding as they are in injection molding | The equivalent failure is a pinch-off mismatch, fixed at the pinch-off |
Wall thickness and part weight are checked on the line, and critical dimensions are measured against the drawing. A material test report and a certificate of conformity are issued per lot, so the resin behind a delivery traces back to the batch it came from. For food-contact parts we can provide FDA, EU 10/2011 and LFGB documentation on request: tell us the market the part has to clear and we will tell you which files we can issue for your grade.
Parts are bagged and boxed in batches tied to the lot number. Pallets, wooden crates or export cartons are used depending on part size, and the same palletization is used for mold crates, so mold and parts arrive in a known sequence.
A standard blow tool typically reaches first articles in the same 15–25 day window we quote for injection molds, depending on the number of cavities, the neck complexity and the cooling circuit. Send the drawing in STEP, IGES, DWG, DXF, STL or PDF with the annual volume, the target market and the material. We reply with a DFM review and a quotation within one working hour, and the mold belongs to you once it is paid for.
Tell us the market the part has to clear and we will tell you exactly which documents we can provide.
BLOW MOLDING NOTES
HDPE and LDPE for containers, multi-layer co-extrusion, and recyclable PP for the EU. The tool is different too, and so is the cost.