HXNINGBO HENGXIN MOLD

Track your project

FOR EXISTING CUSTOMERS

Track your project,
process by process.

Enter the access code we sent you and check your mold’s machining progress at any time — every step photographed on the shop floor the same day.

SERVICE

Die casting in aluminium
and zinc.

High-pressure casting with CNC post-machining, so the part arrives at tolerance instead of arriving at “cast and trim it yourself”.

SERVICE

Die casting in aluminium
and zinc.

High-pressure casting with CNC post-machining, so the part arrives at tolerance instead of arriving at “cast and trim it yourself”.

A380 / A383Aluminium
ZAMAK 3 / 5Zinc
±0.05mmAfter machining
CMMEvery batch
Process Equipment What it means for your part
Aluminium casting A380 / A383 Lightweight structural housings with good corrosion behaviour and castability.
Zinc casting ZAMAK 3 / ZAMAK 5 Denser, harder, and the usual choice for small precision parts.
Post-machining CNC in house Bored, faced and tapped features cut after casting to the drawing tolerance.
Finishing Deburr, polish, blast As-cast, tumbled, bead-blasted or polished to your surface spec.
Verification In-house CMM Cast and machined dimensions both measured and reported.

Typical die-cast parts

Gearbox and motor housingsPump and valve bodiesHeat sinksAutomotive bracketsLED housingsSmall mechanical parts

Die casting is a different buy from injection molding. Molten metal is injected into a steel die at high speed under high pressure, the die fills in milliseconds, and the part is ejected while it is still hot. That buys short cycle times and a near-net shape, but the mold is a much heavier and more expensive piece of steel than a plastic mold, and the part arrives with the tolerances of a casting unless the features that matter are machined afterwards.

That is why our die casting service is built around CNC post-machining in the same building. A380 and A383 aluminum and ZAMAK 3 and ZAMAK 5 castings are finished here, machined where the drawing demands it, and both the cast and the machined dimensions are measured and reported. We have built molds in Ningbo since 2000, and die casting, the mold shop and the machining sit on one 1,200 m² shop floor.

Alloys we run

Alloy Typical properties Where it usually fits
A380 (aluminum) Good castability, corrosion resistance, light Gearbox and motor housings, heat sinks, structural brackets
A383 (aluminum) Similar casting behavior to A380 with a different fluidity and strength balance Housing covers, thin-wall castings and decorative parts
ZAMAK 3 (zinc) Denser and harder than aluminum, good dimensional stability Small precision parts and thin-wall housings where detail matters more than weight
ZAMAK 5 (zinc) Stronger and more wear resistant than ZAMAK 3, at a higher material cost Gears, levers and hardware that carries load

Mold: die construction, draft and gating

A die casting die is a hardened steel tool with two main halves, a hot chamber that holds the metal, and a gating system that carries it into the cavity. Draft is not optional: typically 1° minimum on external surfaces and 2–3° preferred, and more on surfaces that are textured or polished. Internal cores that withdraw sideways need slides, and every slide adds cost, cycle time and a shut-off face that has to be vented. We design the die around the annual usage rather than around a peak number, so the cavity and the HSF inserts are sized for the life you actually need.

Venting is where most die problems start. Gas trapped behind the fill front shows up as porosity, while a vent that is too large shows up as flash. We vent at the last place the metal arrives, which is normally the end of the thickest section. Ejection is the other side of the same problem: ejector pins leave marks, and a part that is too hot sticks to the core. Radiused corners and even cooling do more for the life of a die than any surface treatment applied afterwards.

Shrinkage, tolerance and what machining buys

Aluminum die castings typically shrink by around 1–2% depending on the alloy and the wall thickness, and zinc alloys shrink less. Cast features therefore need the shrinkage compensation built into the cavity, and a dimension that has to be held to a tight tolerance is normally machined rather than cast. As-cast tolerances usually sit in the region of ±0.1–0.3mm on general features, depending on the size of the feature, while machined features can be held to ±0.05mm or tighter, and that is the figure we quote and verify on the CMM.

Shrinkage compensation is also why the drawing matters. Mark the dimensions that are critical and say which ones may be left as-cast, and that single note usually removes a machining operation, a handling step and a cost from the quotation.

Common defects and what causes them

Symptom Typical cause What we do
Misrun or short shot Cold shut from a cold die, trapped air, or a slow fill Warm the die, open the vents, check the shot profile
Gas porosity Air trapped behind the advancing fill front Vent the last point of fill and reduce turbulence in the runner
Shrinkage porosity A thick section solidifying before it is fed Move the feed to the heavy section and rebalance the local cooling
Flash Damaged die face, excessive shot pressure, or a worn shut-off Repair the die face and check the fit of the slides
Sink marks A heavy local mass with not enough feed behind it Rework the wall thickness and improve the local cooling
Cracking after ejection Ejector stress, sharp corners, or uneven cooling Radiuse the corners, even out the cooling, adjust the ejection
Die soldering Aluminum alloying onto the die surface Adjust the die chemistry or the surface treatment and plan a die repair
Warpage Uneven cooling or uneven ejection force Balance the cooling and align the ejectors

Post-machining, finishing and verification

As-cast surfaces are deburred, tumbled, bead-blasted or polished to the finish you specify. Bored, faced and tapped features are cut on our CNC machines after casting, so a bore is a real bore with a real tolerance rather than a cast hole dressed by hand. Cast and machined dimensions are both measured, and the report travels with the shipment.

DFM points we check before quoting

Sampling, lead time and shipment

First articles are shot from the die on our own machines and sent to you with a dimensional report before the die is finished and released. A standard die typically reaches first articles in the same 15–25 day window we quote for injection molds, with slides and complex cooling sitting at the long end of that range. Die cast tools are heavy, so the tool ships in a wooden crate with the inserts and the die shoe packed separately where that is practical, and the shipment documents list the alloy, the lot, and the maintenance and coating instructions.

Send the drawing in STEP, IGES, DWG, DXF, STL or PDF with the alloy, the annual volume and the tolerances that matter. We reply with a DFM review and a quotation within one working hour, and the tool belongs to you once it is paid for.

Send the drawing or the part.

Give us the alloy, the wall thickness and the tolerances that matter – we will tell you what casting can and cannot hold.

REQUEST A DIE CASTING QUOTE →

DIECASTING NOTES

Die casting is a different buy.

Aluminium and zinc have their own molds cost and lead time. Before you compare quotes, it helps to know what sits inside a die casting price.

What an injection mold costsHow long an injection mold takesFiles needed for a quotation

WhatsApp us